Soft PU Foam Material Testing Data

Low density / easy to occurs cleavage and produce the yellowing phenomenon by the ultraviolet light / it is obvious to produce the yellowing phenomenon which the non-adding anti-yellowing agent of soft foam after exposing to ultraviolet light / with the good anti-yellowing property after adding the product. 

Description

Soft PU foam material

Low density / easy to occurs cleavage and produce the yellowing phenomenon by the ultraviolet light / it is obvious to produce the yellowing phenomenon which the non-adding anti-yellowing agent of soft foam after exposing to ultraviolet light / with the good anti-yellowing property after adding the product. 

Variable fade testing laboratory

Sample Size: 200mm thick soft foam TDI Base

Test temperature: 50 ℃

Add amount: 2%, 3% GGK-690

Measurement Unit: yellowing index

Foam density: 0.03 ~ 0.05 g / cm3

Test time: 24hrs

 

The experimental results

Add 2%, 3% GGK-690 provides a soft PU foam material good light performance make foam yellowing change value to 15.2 and 10.79, representing 29.2 is better not to add foam.